Springtime is upon us and a lot of folks are finding minor cracks and holes in their fiberglass boats. Of course everyone wants to get these repaired in time for the first warm weekend of boating. Chapter 2 of our Fiberglass Boat Repair & Maintenance manual shows how to make these kinds of repairs, so we're reprinting it here. You can download the entire Fiberglass Boat Repair & Maintenance manual here.