Estimating the number of reinforcing fabric layers

To determine the number of fabric layers required to achieve a specific laminate thickness, divide the thickness desired by the Single Layer Thickness of the tape or fabric you intend to use.

Product number 740 742 713 702 729 745 737 738
Fabric weight 4 oz 6 oz 11 oz 11 oz 9 oz 12 oz 15 oz 22 oz
Single Layer Thickness * .008" .010" .012" .015" .017" .020" .033" .040"

* Average of multiple layers applied by hand lay-up