Fence and gate construction


Rot is one of the major disadvantages of a wooden fence. Wherever there is a fastener—nail, staple or screw—there is a potential site for rot to begin. Water gets around each fastener and soaks into the wood. When the temperature and the moisture content are right, rot invades these areas. To make a fence that would not rot quickly, I used a rot resistant wood and eliminated fasteners, gluing pieces together instead of nailing. Not only was the process fast—I could assemble 42' of fence a day—but warps and twists in the fence material were easily dealt with.

Our local lumberyard stocks construction grade cedar 2x4 and 2x6. I bought a stack of each and began by machining the spindles—240 of them—at my shop. I ripped them so they had a cross section of 1-1/2" square. Next I cut them to length, cut a chamfer on one end, and sawed a shallow dado as an accent feature.

 

Starting with a jig
  To build the fence, I needed a method of quickly aligning the spindles so they were parallel, had consistent spacing, and had good alignment along the top. To accomplish this, I built a jig to assemble the fence sections. The jig consisted of two sheets of Oriented Strand Board (OSB) with a series of spacers screwed to each sheet. I made the spacers with scrap stock left over from making the spindles and spaced them 1-1/2" apart—the same dimension as the spindles. The two sheets of OSB were placed end to end so I could build 16' sections of fence.

Once I had all the spacers installed, it was easy to lay the spindles between the spacers and at the same time align the bottom edge of each spindle flush with the edge of the OSB. This automatically aligned the height of each spindle. The good side of the spindles was placed face down on the jig.

  Using the 2x4’s for stringers, I laid them across the spindles and marked their location on each spindle. I moved the 2x4’s out of the way, mixed some WEST SYSTEM® 105/206 with 403 Microfiber to a mayonnaise consistency, and put a glob of the thickened epoxy where the 2x4’s crossed each spindle. When I had the globs of epoxy in place, I set the 2x4’s in place and weighted them down until the epoxy cured. No screws were necessary to anchor the 2x4’s to the spindles.

I used the "cake decorator" technique to apply the thickened epoxy to the spindles. I mixed the resin, hardener and filler to the appropriate consistency and dumped it into a Ziploc™ plastic bag. I sealed the top of the bag, snipped a corner off the bottom and squeezed the material onto the spindles. The amount deposited is controlled by the size of the cut corner.

When the epoxy had set, I lifted the fence section from the jig and carried it over to the 4x4 posts that were already in place. I mortised the posts to accept the 2x4 stringers and glued the posts and 16' section together. Then back to the fixture to build another section. Because the temperature was very warm and the epoxy cured quickly, I was able to build several sections a day.

Epoxy for gate construction
Epoxy can also be used to avoid stesses often associated with gate construction. If nailed, screwed or bolted together, the gate pictured would only last a year or two. The stress on the fasteners would begin to crush the adjacent wood fiber and elongate the hole. Eventually, the fasteners would begin to wobble in their holes and make the problem even worse. To avoid the problem, this gate was glued together. The large surface area in each joint distributes the loads and alleviates the point loads that are the downfall of metal fasteners in relatively soft wood.

The boards that form the starburst pattern provide the strength to keep the gate from sagging. The long boards in the starburst are being pulled lengthwise, wood's strongest direction. The shorter boards are being compressed, but, because they are short, they are not as easily bent as longer boards would be. The large gusset in the upper hinge corner of the gate distributes all the stresses over a large area.

Once it was properly engineered, building the gate was easy. It is a sandwich consisting of two rectangular layers, one on each side of the starburst pattern. One layer of the outer rectangle was cut and laid out on the floor. The starburst truss parts were laid on top of the rectangle and bonded to it. WEST SYSTEM epoxy was applied to both surfaces using the two step bonding procedure and the process repeated to bond the top rectangle. A little light clamping pressure was applied to the joints until the epoxy cured.

To complete the assembly, hinges and a latch mechanism were installed. Because the weight and leverage of the entire gate were concentrated at the hinge fasteners, these were good candidates for hardware bonding. As we pointed out in the last Epoxyworks, wetting the fastener pilot hole with epoxy doubles the pullout strength of the wood. Drilling an oversize hole and casting epoxy around the fastener will, at a minimum, triple the pullout strength.

Side loaded fasteners also benefit from being installed in an oversize, epoxy-filled hole. Epoxy around the hinge bolts better distributes the loads placed on them into the wood, and, as a bonus, the epoxy annulus keeps water out of the fastener holes.

Epoxyworks 14 / Fall 1999

Epoxyworks - View our Epoxy Magazine Online SCFB       facebook    twitter   YouTube

WEST SYSTEM is a registered trademark of West System Inc | Sitemap | Terms & Conditions | Web Site by Ingenex Digital

Customers in Europe, Africa and the Middle East may be best served by West System International