Saving The Deck

There are often interesting articles in Epoxyworks magazine illustrating the different uses of the WEST SYSTEM epoxy. I admire the time and effort that goes into some of these handmade boats that are like art projects. But in my particular situation, I was most concerned about strength rather than the aesthetics. I was dealing with wood rot at the bases of the support posts for a large patio deck. There are two levels on this deck, with the patio furniture on the top level and a built-in hot tub in the lower level. The deck is constructed of 6×6 support posts, 2×12 flooring supports and 2×4s for the finished floor. All of this is redwood.

Blackmon's two-story deck is supported by 6x6 redwood posts
resting on concrete footings.

Last spring after power-washing the deck, I began the once-every-three-or-four-years jobs of staining it. This deck is twenty years old now but still holding up well. But as I applied the stain to the 6×6 support posts, I noticed severe wood rot in some of the posts. Over the years I’d neglected proper landscaping around the base of these, which lead to soil surrounding the bottom two or three inches of the posts. This in turn held the moisture near the footings much longer than it should have. The resulting compromise of structural integrity had to be addressed. In some cases, up to 25% of the cross-section of the post had rotted away. My options were to replace the 6×6 support posts, or structurally repair them. I chose to repair instead of replace.

I cleaned out the wood rot as much as possible using a screwdriver and sometimes just getting my fingers into the voids and pulling out the dead wood. Then I used a wood preservative solution of copper napthenate (green preservative) to halt the rot’s progression. This solution is a spray, but I also poured on directly when possible. This is one of those situations where more is better.

Using an expendable plastic sign, I built small forms to fit around the base of the posts.Each form was 2"–4" high based upon the wood rot on the posts. My idea was to pour a replacement base that enclosed the rotted section of the post, and then some of the remaining post. I sprayed the plastic forms with silicone spray in hopes of an easier removal process. Then I carefully taped them to the original cement footings to hold the poured epoxy inside of the form.

Two of the posts that rotted where their bottom ends rested on footings.  Soil held moisture
against the bottom of the posts creating an ideal environment for rot.

I mixed WEST SYSTEM 105 Resin with 206 Slow Hardener. This gave me plenty of time to get the epoxy into the forms. I thickened the mixture with 403 Microfibers, which made it much easier to contain in the forms. Before removing the plastic forms, I let the epoxy cure overnight.

The forms came away from the epoxy with a little work, but the ink from the plastic stayed with the cured epoxy.This wasn’t an issue since my next step was to paint the epoxy bases so they blend in with the garden around them. I used a dull brown paint that was created for camouflage work to hide the glossy look of the epoxy. 

After treating the posts with wood preservative, Blackmon used plastic sign material to make forms around the base of the posts. The form were removed from the cured epoxy revealing the ink that transferred from the inside of the form to the epoxy. Blackmon finished the repair with a coat of dull brown paint to camouflage the epoxy base.

Lessons learned

It is not worth the time or effort to sand the epoxy bases. Any finish work needs to be done with hacksaw or grinder. No matter now careful a person is, there always seem to be leaks in the forms. Use plenty of tape to seal the forms, and then tape some more.

The use of epoxy and 403 Microfibers helps immensely when trying to keep the mixture in the forms. All in all, this turned into a very successful repair of the deck with the use of WEST SYSTEM epoxy. This maintenance project should provide another 20 years of life for this deck, and at a significantly lower cost than replacing eight 6×6 support posts ranging from 4' to 16'.

 

 