Storage / Shelf Life

Store at room temperature. Keep containers closed to prevent contamination. With proper storage, resin and hardeners should remain usable for many years. Over time, 105 Resin will thicken slightly and will therefore require extra care when mixing. Repeated freeze/thaw cycles during storage may cause crystallization of 105 Resin. Warm resin to 125°F and stir to dissolve crystals.

Hardeners may darken with age, but physical properties are not affected by color. After a long storage, verify the metering accuracy of the pumps and mix a small test batch to assure proper curing.