407 Low-Density

407 Low-Density filler for epoxy
407 Low-Density

407 Low-Density is a blended microballoon-based fairing filler for WEST SYSTEM Epoxy. Add 407 to a mixture of epoxy resin/hardener to create a fairing putty. It’s easy to sand or carve this putty once it has cured. Low-Density Fairing Filler filler is reasonably strong on a strength-to-weight basis. You can blend it into any WEST SYSTEM 105 Resin/20X Hardener combination, G/flex Epoxy 650, or G/5 Five-Minute Adhesive. Blended with epoxy, it will cure to a dark red/brown color.

Color: dark red-brown.

407-5 Low-Density filler for epoxy
407-5 Low-Density, 5 oz

407-15 Low-Density filler for epoxy
407-15 Low-Density, 12 oz

407-B Low-Density filler for epoxy
407-B Low-Density, 14 lb

Filler Selection Guide

407 Low-Density Safety Data (pdf)

 

VIDEO: Adding Fillers to Epoxy.

Visting Epoxyworks to read about how 407, our microballoon-based fairing filler, is used in repairing machined holes in fiberglass.