CURE TIME:
Working time (thin film) is based on which hardener you choose at 72°F (22°C):
- 205 Fast Hardener®: 60 to 70 minutes
- 206 Slow Hardener®: 90-110 minutes
- 207 Special Clear Hardener®: 100-200 minutes
- 209 Extra Slow Hardener®: 3-4 hours
CURE TEMP:
Based on which hardener you choose, solid-state curing happens in a wide range of durations at 72°F (22°C). Minimum recommended temperatures:
- 205 Fast Hardener®: 40°F (4°C)
- 206 Slow Hardener®: 60°F (16°C)
- 207 Special Clear Hardener: 60°F (16°C)
- 209 Extra Slow Hardener®: 70˚F (21˚C)
PRODUCT SIZES:
- 105-A: 1 quart
- 105-B: .98 gallon
- 105-C: 4.35 gallon
- 105-E: 52.03 gallon

105 Epoxy Resin Facts