STRENGTHEN COMPROMISED WOOD WITH CONFIDENCE.

 

New from WEST SYSTEM® Epoxy, the Wood Rot Repair Kit provides a cost-effective and time-saving solution for making repairs to rotted wood. This two-part, solvent-free epoxy system penetrates deep into damaged areas, consolidating weakened wood fibers. It’s formulated to be flexible enough to move with the wood’s natural movement, preventing issues from cracking.

Whether you’re fixing up a boat, windowsills on your house, or delamination on your RV, count on Wood Rot Repair Epoxy to reinforce and stabilize rotted wood for years to come.

  • COMPATIBLE WITH FILLERS
    • When mixed with WEST SYSTEM Fillers, it creates a thickened epoxy perfect for filling large voids or rebuilding missing sections of wood.
  • PREVENTS CRACKING
    • Designed to have a bit of flex, Wood Rot epoxy accommodates natural wood movement without cracking.
  • 100% SOLID
    • Wood Rot Epoxy is 100% solid, meaning it’s formulated without solvents. Other penetrating epoxies containing solvents are susceptible to shrinkage and may cause unwanted voids, making your repair less structurally sound.

INSERT VIDEO TITLE HERE Video

This comprehensive overview shows you how to stabilize damaged wood using WEST SYSTEM Wood Rot Repair Epoxy. Watch Now!

WEST SYSTEM Wood Rot Repair Kit (1.5 QT) product image showing resin, hardener, and repair kit packaging.

PROJECT USES:

  • Wood components
  • Home exterior
  • RV repairs
  • Marine
  • Decorative trim
  • Woodworking

CURE TIME:

When working in a 72°F (22°C) environment:

  • Working time: 30-40 minutes
  • Recoat time: thin film: ≥ 12 hours. Surface build-up: 3 hours
  • Time to sand: 24 hours

CURE TEMP:

  • Recommended temp: 72°F (22°C)
  • Minimum temp: 50°F (10°C)

PRODUCT SIZES:

  • Small kit (12 oz.): 8 oz. resin, 4 oz. hardener
  • Medium kit (1.5 qt): 1 qt. resin, ½ qt. hardener
  • Large kit: (1.5 gal): 1 gal resin, ½ gal hardener