PROJECT USES:
- Marine
- Boat Repair
- Bonding
- Fabrication
- Barrier Coating
CURE TIME:
- Pot life (100 grams cupful):
- At 72°F (22°C): 40 to 50 minutes
- Working time (thin film):
- At 72°F (22°C): 3 to 4 hours
- Solid state:
- At 72°F (22°C): 20 to 24 hours
CURE TEMP:

PRODUCT SIZES:
- 209-SA: 0.66 pint
- 209-SB: 0.33 gallon
- 209-SC: 1.45 gallon
- 209-SE: 17.34 gallon
209 EXTRA SLOW HARDENER Facts
QUICK LINKS Helpful Tips, Safety Guidelines, Manuals, and More:
UNCONTROLLED CURE
Controlling exotherm (the heat released by the chemical reaction between resin and hardener that cures epoxy) is very important, especially when mixing larger batches of resin and hardener. If not controlled, epoxy’s exothermic reaction can be dangerous.